Fibreglass & carbon

Repairs that disappear

Hull damage, cracks, wet core or tired gelcoat, fixed properly, layer by layer, and finished so you can’t tell where the damage was.

What we fix

Common fibreglass problems

Some damage is obvious. Some hides under the gelcoat until it gets expensive. These are the problems we see most.

01

Impact damage

Collisions, groundings and knocks against the jetty that crack or hole the laminate.

02

Stress cracks

Spider and hairline cracks around fittings, corners and hard spots. Often a sign of flex.

03

Gelcoat chips & crazing

Chips and fine crazing that look cosmetic but can let water into the laminate.

04

Delamination

Layers of the laminate separating, leaving soft or hollow sounding spots when tapped.

05

Wet core

Water soaked into the core through old fittings or cracks, making the deck or hull spongy.

06

Osmosis blisters

Blisters below the waterline where moisture has worked its way into the laminate.

Fibreglass repair

A repair that’s stronger than the damage

A quick patch hides the problem. A proper repair rebuilds every layer of the laminate. Tap through each stage to see what goes into it.

Beyond repairs

Carbon fibre & custom parts

Carbon fibre is lighter and stiffer than glass, and it needs care to repair properly. Morgan works with both, matching the original layup so the repair performs like the rest of the boat.

The same skills go into custom fibreglass parts: hatches, consoles, boxes and one-off modifications made to fit your boat.

Got a ding, a crack or a project in mind?